I used a new CC PS that I bought. With a CD of 6. Two of the parts were threaded into the rack on both sides of a length of aluminum wire, the other two were wrapped with titanium wire. I used a multimeter to check the voltage on the wires connecting the pieces and it was the same as what the PS was putting out.