View Single Post
  #5 (permalink)  
Old 01-08-2006, 05:38 PM
PDX_Customs PDX_Customs is offline
Newbie
 
Join Date: Aug 2005
Posts: 15
PDX_Customs
Default Re: Won't take dye, need suggestions

Yea, did everything exactly like instructions say, degreaser at 150 degrees for 5 minutes, rinsed and it passed water break test and then did de-oxidizer at 100 degrees for 3 minutes. Rinsed again and put in anodize. Another thing that i forgot to mention is the it has been maybe a month or two since I set up the anodize tank and haven't used it since then, I noticed that the water level had dropped so I added more water to bring it back up, does the acid evaporate too? Should I be adding more acid also?

Thanks a lot