Won't take dye, need suggestions
View Single Post
#
7
(
permalink
)
01-08-2006, 08:24 PM
sswee
Moderator
Join Date: Nov 2004
Location: close to Austin, Texas
Posts: 1,240
Re: Won't take dye, need suggestions
Had the part been stripped of any possible coating. If it had an anodic coating or other type, it would give the results you got and 3 minutes in deox would not have taken it off.
SS