This does not line up just right, will see if I can fix infrared radiation reflectivity (emissivity) of some common materials:, maybe thsi will help you


Material Reflectivity
Aluminum Bright 90-95%
Anodized 45%
Oxidized 70-80%
Brass Bright 97%
Oxidized 39%
Chromium Polished 92%
Copper Bright 95%
Oxidized 22%
Steel Polished 45%
Oxidized 15%
Nickel Polished 95%
Oxidized 5%
Zinc Bright 77%
Oxidized 77%
Paint White 10%
Black 14%
Rubber 6%
Water 8%