AH I see does the ground loop back to the gun in most setups? that would make a good circuit.

Before I start still wondering about anything touching the sprayed areas. Is hanging from a non sprayed area the only or best way to go? if so I will need to make an oven as it looks like many of you have i.e. a 17" wheel wont fit in most ovens Ive found