Learning how to polish i'm doing a Turbo housing for a buddy. This is about the third thing I have ever polished(and hardest thing also). I'm fairly happy with it to be honest. I feel I could do a lot better in the tight areas once I get the right equipment.
My question is around the wording is it "ok" to leave it like that with the pitting?(hard to see in the pics but there is some there) Is minimal pitting around lettering normal? It seems it would take me forever in a day to get rid of it...even after I order some abrasives for tight areas.....
I did 180 greaseless
320 greaseless
Tripoli on a treated wheel
Color on a soft cotton wheel.
Sounds easy but it took HOURS. I guess I have some refining to do. I just found this site and plan on ordering some abrasives for the tight areas....