Effectiveness of a wheel depends on the machine it is on. The RPM X circumference = FPM. On my machines I use 6" wheels down to about 4" then set them aside to be used on hand tools. If your wheels start out at 10", you should be able go down to just below 6" or so. You should be able to tell when it's not working as well as it was. I just keep extra wheels on hand so I don't get caught waiting for new ones to arrive. after you do it awhile, you'll get the feel for it.
Prep for clearing is the same as any paint. you just want it as clean as possible.