Yellow Chromate & Copy Cad
Hi. I had the kit for about three weeks now, it is still awesome. Have absolutely no complaints, praise only. However, I was under an impression that Yellow Chromate will dye even commercially obtained zinc plated items. I tried to "yellow" some nuts and bolts from a local hardware store, the color seems to be right, but the yellow finish can be rubbed off with a shop towel (24 hours later)! The items were properly degreased and I tried some battery acid on them, zinc reacted very rapidly. What am I doing wrong? I must note that my freshly plated parts accept Chromate well and finish seems somewhat durable, still VERY easy to remove the yellow coloring with steel wool. My chromate solution is applied for two minutes at 22 deg. Cel. Thanks.
Andrew.
|