View Single Post
  #4 (permalink)  
Old 03-03-2003, 07:28 PM
newman newman is offline
Newbie
 
Join Date: Mar 2003
Posts: 1
newman
Default

i too am having a hard time getting the yellow chromate to hold, right after i zinc plate i rinse with water and dunk into chromate for about 1-2 mins ,after 2-3 days i can remove all the color off with water and a rag, im running the bath @80%.... any ideas how to resolve this?
would a Nitric Dip help right before chromating?

thanks .

ps: im zinc plating old carb castings from the 60s.