Thread
:
gloss killer not so killer?
View Single Post
#
7
(
permalink
)
02-09-2006, 06:28 PM
jtagger19
Experienced Metal Finisher
Join Date: Apr 2004
Posts: 466
Re: gloss killer not so killer?
if you are talking about the satin clear
you don't mix it with color
it a satin clear
you just apply it as a normal coat after the color
jtagger19
View Public Profile
Send a private message to jtagger19
Find all posts by jtagger19