you can get mineral wool which is used in furnaces from McMaster-Carr. We just built a 4X4X6 oven using 2" of 1800 degree insulation---cool to the touch on the outside when running at 400 degress

Ed
Have pics of ove email me and i will send, can also provide part numbers of all the items used in our oven!!