What I have so far is 4 - 3000 watt elements for a 3 x 3 x 6 oven based on 60 amps and 220V
1. What size of contactor do I need and the poles? A link would be great.
2. Cheap digi control with thermostat for 220V? A link would be great.
3. Anything else?
Yikkees! I hope im not gettin in over my head....
Thanks!!!!
__________________________________________________ _____________
1.-if your running 220V 2 pole contactor
2.-$188 for a digital control from McMaster..use one side of the 220V line to power the controller..make sure you get the one that runs off 90VDCto240VDC or you will need a transformer-McMaster part# 38615k11
3.-email me for pictures of mine:
whome124@aol.com