Default Re: Vibratory Aluminum Polishing

Interesting was also thinking along the same lines as yourself - get great results with the buffing wheel and Walter Blue Mirror Finishing Paste - not really a paste though - it is a solid (of course until it is heated) - did discover that it is easily crushed and ground. So that is on the list of experimentations, so combine that with a soft media - and well we shall see!

Later,

- Jon