have had my system for a few weeks and have plated a lot of parts anyway I have found to obtain the finish you are looking for it sounds like you need to increase the power for fasteners such as 3/8 I first run them through the tumbler then I plate at .50 to .65 amps and will get a part that looks like chrome. just try a higher amps there should be just a small amount of bubbles frrom the part.