Re: Copy Cad Plating Questions?
Here is my preparation process:
First dip in acid until all the oil zinc is gone
Rinse in DI water
Dry
Polish with a wire wheel
Dip in acid for a couple of minutes
Rinse
SP degreaser
Rinse
To plating bath
If my parts where preped poorly wouldn't the zinc fail to adhere? The zinc seems durable. Is there a film on the freshly plated parts that causes the chromate not to adhere?
I have been going from the plating bath to a rinse then directly to the yellow chromate.
Thanks for any advice, Ross
|