Default Silver polish on 24k gold plate??

I just came across a large supply of silver polish CHEAP!

Tarni Shield silver polish,
Anti tarnish protection from the makers of Scotchgard protecters.
A 3m product.

Says special anti tarnish protecter, not a laquer.

It is recommended for about anything silver! Is there any known reason not to use this on 24k gold plate?

I had some very brown 24k gold plated test pieces, shined them up with this silver polish. The pieces now sparkle and shine like gold

Been a few days or more, and they still look great. Using a dab of polish on a cotton ball with very light rubbing was all it took.
So far it hasn't caused the gold to turn green or peel or anything, so do ya think it is safe to use on good stuff?

I wouldn't be so cheap, but I got a nearly life time supply nearly free, and since I have it....
Also I don't have any gold polish!

If this will work good with no side effects I'd rather buy more gold solution than a bottle of Flitz. I'm almost out of gold