Default Re: Refrigerator Oven Help!

try to find a way to put a fan in there and that will go a long way to solving the problem. as for relocating the element i would not at this point till you get the air moving it may be fine where it is. remember that heat rises so the top will always be hotter than the bottom so install the fan on the top to push the hot air down.
__________________
when in doubt polish it out/ why replace it when you can refinish it