Hey SICKGIXX.
I also have the same problem after the weld to the lower part of the frame. Ive noticed that it seem to be getting a little bettereach time i sand. I also sanded my frame 3 times on the lower half. 180 to 2000. I think that the pot marks are still there tough, and still have some anodizing left it in them. Im going to try a heavier duty paint stripper and see if that pulls out anything. Other than that, I believe that more sanding is involved. Have you had any luck in the past few days.
Troy