NeoMoses,
Nickel acetate (anodize sealer)is available in 2 flavors that I know of. One has to be heated to boil or all most boiling, and the low temp, which works around 90 degrees. Anodize sealer is faster and easier that boiling water or steam. The 190 deg mentioned in alt.rec.metalworking is that standard sealant.
|