Default replating a bike fork crown

Hi, I am restoring a 30 year old bicycle. It had a chrome fork crown, but most of the chrome had peeled off over the years, leaving (I assume) a nickle plating over steel. I have polished what's left of the old finish, and it looks ok, but I'm hoping I can replate the fork crown, and maybe some other small areas of the frame without too much trouble...
I just ordered the chrome dip kit for $30.00, and am wondering if anyone has any hints, I haven't received the kit so I'm new to this idea. Thanks