Quote:
|
Originally Posted by sswee
If it's leaving marks in the bar, it's loading. New wheels don't load real good and you have to load more often till they become seasoned you might say. After a bit of use they will load faster and stay loaded a little longer.
SS
|
that is it exactly. it takes a few runs on a wheel to get it to hold conpound. also flannel may be a little to soft for what you want. if so move to a loose cotton.