I have a CASWELL LCD system that I'm setting up. The CASWELL manuel says to mix the battery acid at a 3 part distilled water to 1 part acid, I have read elswhere that you should use a 1 to 1 mixture, which is the proper mixture to use? I have a used Astron VS-35m power source that I plan to use on my 5-gal set-up.