Re: shocker surface area
Ha, I think I already answered you in the PBN forums.
Body: 62 sq. in.
Gripframe: 38 sq. in.
As for the rest of the dimensions... maybe someday.
But this brings up an interesting subject that a local Profesional anodizer and I discussed recently... CV anodizing where you don't have to measure the surface area. I'll start a new thread on that subject.