View Single Post
  #1 (permalink)  
Old 03-15-2006, 01:43 AM
blacklincoln blacklincoln is offline
Newbie
 
Join Date: Mar 2006
Posts: 8
blacklincoln is on a distinguished road
Default stainless trim polishing taking forever..

i am restoring a 63 lincoln with miles of stainless..
ive been working on the smaller parts first using a da sander with grits from 320 to 1500 then move to a spiral wheel with emery..
problem is the wheel takes forever to get the sandpaper scratches out...i could spend 2 hours on a 2 foot long trim piece and it still wont be perfect..

heres my pile of homework..minus two 4" x 5 foot rocker panels..and fender trim..

i just ordered the sisal wheel and the f515-6154 and f515-6147 compounds should this solve my problems??...


i was also wondering about this thread...could it possibly be that easy to remove the chrome/chromium plating that it on these lincolns..i just cant believe a chemical could remove the outer plating without harming the stainless underneath..right now i am sanding off the outer layer and that step actually doesnt take too long with 320 on the da sander..but still am looking for an easier route if possible..
Chrome on stainless steel