Quote:
Originally Posted by callmej75
I always thought it was a rule of thumb to bake the base coat at 1/2 the cure cycle then bake the top coat at full cure cycle to make sure no "over baking" occurs on the base coat?
I've heard that you know I've read so much on here. I guess you just have to figure out whats best for you. If it screws up don't do it that way no more. LOL LOL