03-19-2006, 07:52 PM
m67bd70x
Newbie
Join Date: Nov 2004
Posts: 24
Re: is galv sheet metal safe to use?
I've had no problems yet. But you are correct, welding galv does produce fumes that can be hazardous to your health.