What I found was that when I first got it I wasted alot of powder getting it setup. Once I got used to the gun and the way it works I was able to adjust it very quickly and increase the transfer efficiency and now find that I'm using less powder to do most jobs. As a nice side effect I'm also going though fewer filters in my booth. I don't do any production work so I almost never need to refill the cup, but each job I do I'm also pouring less powder than I did in the beginning. Basically I would use something like 2 lbs to do 4 wheels, and now I'm using a little over a pound.