Re: Oven Metal
Our oven is sheathed inside and out with 20 gauge galvanized, no problems or toxic fumes. I did a burn off at 400 for an hour to make sure, works great for us. The main thing is the air circulation for hot/cold spots. Other then that galvanized is fine, alot of larger ovens are built using the same material.
Ed
|