Bud what’s up ?
Man ill tell you what a lot of big plating shops don’t even do pot metal and if they do some of the turn around is unbelievable like 6 to 8 weeks and the price ouch !!! you might call and talk to Craig ext 114 at Caswells there are some products that make the job a little easier but really this is one of the biggest problem metals even the large shops that do plate pot metal don’t give any typ of wnty . This is the reason shops like yours and mine are swamped with it the second I told people I was set up for pot metal oh man .. But im like you just a one man shop I have over 150 pieces to plate and more then half is pot metal ..
__________________
Jim Eaton

Last edited by jimcarry; 03-22-2006 at 08:03 PM.
Reply With Quote