a) While sandblasting (aluminum oxide) an aluminum intake, I noticed many, many black dots being penetrated into the material. Why did this happen, how do I avoid it and can I repair the intake?
b) After blasting two steel brackets, cleaning with dish soap, pre-heating, coating and letting cool in the kitchen style oven until back at room temperature I now have tons of tiny black dots visible throughout the brackets. Please advise on what you think may have caused this and how to prevent it.
c) I researched outgassing and understand how to avoid it, but I can't figure out what "faraday" means.
d) Please recommend a gun system around $1500 (or less ), I plan on strapping a pound or so of TNT to my Chicago Electric system when I get the new system! One of you guys recommended the Caswell portable system, I would love some more input on other guns and reasons.
e) How are you guys getting oil out of engine parts like valve covers after power washing at the local car-wash (not that I would ever do that )? I wouldn't mind spending some money on a good system, as I plan on focusing on engine parts.
f) I have purchased 10 or so different colors and types of powder off e-bay and unfortunately don't know how to determine if they are of good quality. Please recommend type and supplier for engine parts. I also have some motorcycle parts that will be exposed to UV and fuel, grease and grime- what do you recommend for these type parts?

I truly appreciate all your help. I have read everything I can get my hands on and want to do well with this. I have built a nice paint booth, spent some money on my air system and bought different types of abrasives. I have succeeded with a few parts thus far, but don't want to continue doing things wrong. Thank you thank you thank you!