First off let me welcome you to the Forum
Temp plays a big part in all plating as well as agitation .
The rust you are talking about could be just not complete coverage or that you don’t mention using any typ of protectent after plating these things all play a large part of the plating process
also and I cant say this enough but preparation is everything.