I just run my first test using the output of my new caswell RO Unit(thanks guys) in conjunction with a Deionization(DI) filter. The DI water improved the quality of the zinc coat a slightly on a steel wrench while giving a significant improve on zinc die-cast substrates. This might be due to a local quirk in my ground water, or it might work for others

.