I see. I thought you wanted to anodize it.

You give it a brushed look by polishing it with a wheel like our brightex wheel. You can then plate it with Copy Chrome. It won't look shiny, it will look like a brushed aluminum finish.

The surface of the metal before you plate (or anodize) dictates the end result. Polished parts in come out shiny. Dull/brushed parts in come out dull.
__________________
--
Mike Caswell
Caswell Inc
http://www.caswellplating.com
Need Support? Visit our online support section at http://support.caswellplating.com
Have A Web Site?
Why not join our affiliate program and earn 15% of all sales. Join at http://www.caswellplating.com/affiliate.htm
Reply With Quote