View Single Post
  #33 (permalink)  
Old 03-26-2006, 10:04 PM
KZjim's Avatar
KZjim KZjim is offline
Amateur Metal Finisher
 
Join Date: Oct 2004
Location: Cereal City - There's a lot of flakes here
Posts: 132
KZjim is on a distinguished road
Send a message via Yahoo to KZjim
Default Re: aluminium motorcycle wheels - pc'ing cause failure?

machone.. my thoughts exactly, if heat effected it, the simple act of welding it would do damage to the properties of the material.
Back to the subject at hand.. i also sent an email to the NHTSA to see if they have any data on this subject.
__________________
If it jams; Force it. And if it breaks it needed replacing anyway.

I can go from 0 to "What seems to be the problem Officer?" in 3 seconds."
Reply With Quote