sweet thanks for the support. And Mike you can be sure that I will be asking some questions. And I am pretty sure that it is going to be single phase and Im thinking of building it the same way as you Mike, except mine would lay on the ground and be 6' long instead of high. So are the 4 1500W elements enough to heat that up? Also how thick are your walls. Is 1inch thick insulation enough are is it better to go with 2inch thick?