View Single Post
  #21 (permalink)  
Old 03-27-2006, 01:24 AM
-AAPB-Eric -AAPB-Eric is offline
Amateur Metal Finisher
 
Join Date: Mar 2006
Posts: 126
-AAPB-Eric is on a distinguished road
Default Re: CV anodizing and electrolyte Titration

Just to give you a heads up-

Spoke with AF for a bit, he said its really dependent on the dissolved AL content.





Quote:
Originally Posted by ArmyAntz-Eric
Just have a general question about the tips about CV you gave me on the forums.

I have a 3:1 water to acid ratio and was wondering if this would change the perameters you gave me? I dont have anything titrated and wont for a while so would the calcualtion of SA and the proper calculations work in my favor till I get the titration kit or is this CV method forgiving?



AF- Thats hard to say. Its not that acid ratio that is the issue with CV, its the Aluminum content of the bath. Typically you want about a 10% of dissolved aluminum content in your ano bath to run CV. I dont know what your 3:1 works out to as in Grams per Liter, so I cant weigh in on that.




For now, ill just measure out the parts and compile a list. I wont have any issues sharing SA dimentions.

Last edited by -AAPB-Eric; 03-27-2006 at 01:26 AM.
Reply With Quote