Default Re: clear on polished mild steel

Quote:
Originally Posted by machone
Clear looks great over polished. If you're getting orange peel, I suggest lowering your cure temp and cure for longer. It gives the powder more time to flow.
mach
That's what I do! Along with a slow ramp up to temp. I do this with all of my gloss parts, and it works great!

Doug