Thanks M_D, the object is machined from 2x1 inch 6063 extrusion, wet sanded and polished by hand on a buffing wheel with Caswell Cut and Color compound.
I will try a short custic dip, say 3 minutes, in warm 20% caustic and as see if this improves the result.
|