Thanks Fly
I'll try air to agitate the bath.I understand about the 0.1/amp per sq,in.Do you think I'm okay useing the copper wire for anodes,I basicaly wrap the wire close together around a 4"x6" stainless anode the pull the anode out then tie it.Also Dalmer says to hang the anodes on one side and the part on the other,so I will also try hanging the anodes on both sides.thanx much.