Quote:
Originally Posted by Popeye
You mean it's heavier around the edges... that would make it darker around the edges..
Are you spraying both sides?
If you are, spray the back first and the do the front. It's always thicker around the edges.
Well when I did my first samples when I set everything up, they all turned out great. But I think I found my problem. My samples were suspended too far down....so i shortened the hooks and it cured it a little. I don't have a powder flow setting on my gun so I just adjust the air down to maybe 10psi.