Default why flat finish

I dyed my first test piece but the color came out flat, after anodizing are you supposed to repolish the part to get polished color look? It had a powdery surface that rubbed off easily but still had color underneath. My dye was at room temp and dyed the piece fine. I then sealed in CASWELL sealer that was boiling.The color was CASWELL fast blue. The finish was flat but had good color that rubbed off easy but still had color underneath. The piece was scrap diamond plate (12"x6"x1/4") that was anodized at 6amps for 120 minutes at 14 volts. Can you repolish after anodizing before dying?