View Single Post
  #3 (permalink)  
Old 03-29-2006, 12:56 PM
grommit's Avatar
grommit grommit is offline
Amateur Metal Finisher
 
Join Date: Mar 2006
Posts: 208
grommit will become famous soon enough
Question Re: primary chain cover prep help

hi m8,
i've just replied to your message on the oven cleaner thread and asked about this whilst i was on it...ha ha and you had already answered this.
thanks m8 so its 200 grit,most of the threads i have read is go to 600 and no more,please can you confirm my exact grades you recommend and wet aswell.i've just looked at your chart you give me when i 1st came on but i'm a bit confused
p120= 120 grit us
p320= 260 grit us
p400= 300 grit us
p600= 380 grit us
p1000= 550 grit us
p1500= 800 grit us
p2000= 900 grit us
p2500= 1100 grit us
200 i take it is course and it gets finer or was i just askin an obvious question there.
am i right on the next part
to be honest alot of my parts i could start with cleaning and then straight into spiral/tripoli for the cut(back to sisal/black for worse scratchs)and finish with loose/white for color...would blue be also an option at that stage.i was hoping harbarfreight would get back to me today ref buying a buffer from them..oh well i've waited this far,patients is a fertue so they say....I BLOODY WANT IT NOW..ha ha
cheers m8
bri