1. Dipping in an acid pickle will remove the existing zinc plate. See the section in the manual on acid pickles.

2. It depends what the metal is. If it's die cast, then NO. The acid will attack the part.

3. It should last a very long time. Try plating a thicker layer of zinc.
__________________
--
Mike Caswell
Caswell Inc
http://www.caswellplating.com
Need Support? Visit our online support section at http://support.caswellplating.com
Have A Web Site?
Why not join our affiliate program and earn 15% of all sales. Join at http://www.caswellplating.com/affiliate.htm
Reply With Quote