i have not tried it but would say no it wont work on the pipes. as for the slipon mufflers maybe but not the head pipes. as for the heat shields it should be ok. on my harley it gets hot enough to melt anything that touches the headpipe so i would say it is above 400 degrees and the regular powder would not hold up.