Default Re: expert info

I can garante it won't work
I tried many times it will bubble up and peel off
in fact high temp powder is the only one that I have had good results with and not for a long time
normal temp on a harley bike is 600-700 riding it's higger
only ceramic coat will work
I've done heat covers with no problems