I just received the 4 gal tripple Chrome kit. The Copper crystals say to mix contents of bag with 1 gal distilled water and this should make two gallons. The kit came with two bags but they don't fill the tank to 4 gallons more like 3 gallons. Also the nickle crystals say makes 2 gallons per bag there are two bags but doesn't say how much water to mix. If I add 1 gallon of distilled water per bag it doesn't equal 4 gallons closer to three and the brightner treats 4 gallons. The flash copper and the Chrome fill the tanks to the four gallon mark and a little beyond. So what I am trying to say is the copper crystals mixed per instructions do NOT equal 4 gallons and the Nickle crystals am I to add distilled water till it reaches the 4 gallon point.