Re: specs for a large oven
i think the boxes are used more for mounting than wiring. as a side note most elements that have wires attached will have the high temp silicone jacketed wires on them. if they are stud ended then try to get the connections outside of the hot zone if possible.
__________________
when in doubt polish it out/ why replace it when you can refinish it
G2 Polishing and Powdercoating
|