Smile Re: Help!!!

Thanks for the info, but you must have misunderstood, the parts that I tried to dye Red and Navy would not take those colors, the same parts when I tried them in Teal DID take!!!! This was on the same run,not a re-anodized part. When the parts would not take the Red or Navy, I then put them in the Teal dye and the color DID take, this is why I thought it might be a PH problem.