thanks Sswee, for the catch.
yes--- the amp calculation is very close to the 6 amps stated.
Funny, after reviewing the dimensions I realized it mimics
Caswell's own rule of thumb:
for 1amp = 50sq" = 1 mil = 240'
1amp = 25sq" = 1 mil = 120' this is for a 6amp sq/ft base

Also to consider Fragglerock's results some more:
Given the diamond plate's material makeup I wonder if
he should hold the 6amp base and drop the anodizing time
25% (Mike C.'s comments in the "sticky" post).
Actually, I would drop the anodizing time by 1/2 and
review the results.

Sswee-- I have seen your putters done in the "fast blue".
Is that dye not brought to 130-140dg before use?