Re: question regarding preped parts
Congratulations!
The one part (maybe a paintball gun item?)
looks very trick. Those fades look very nice.
I will answer your Ti wire needs:
Look up Titanium Joe on the internet. Joe
has plenty of Titanium welding wire he can send you.
He has .062 I know, because I just purchased some.
He also has smaller diameters, so just inquire.
archi
|